LPKF presents solutions for industrial printed circuit board production with the new "Single Pico" technology. For the prototype production, the laboratory equipment is presented, which makes a complete in-house production possible. In addition, it demonstrates how the use of thin glass optimizes microfluidics.

Extremely clean cut edges as well as exactly converted geometries are the convincing results when cutting and drilling or material removal with the Single Pico technology with "Cleancut". The heat affected zone (HAZ) of the picosecond laser machined material is so small that it is negligible. With the technology

Manufacturers of high-quality microelectronics can further improve their product quality and make their products even more compact. The manufacturer offers a comprehensive portfolio for prototyping in development departments and research facilities. This makes it possible to realize the entire PCB production in-house. For particularly demanding applications, the machine manufacturer relies on ultrashort pulse lasers.

As a third trade fair theme, the award-winning "Lide" technology offers unprecedented quality prototyping and mass production of thin-glass microstructures for a variety of applications.


Another contribution of the manufacturer This e-mail address is being protected from spambots To display JavaScript must be turned on!

Kipp-Werke
Tretter
Mitsubishi
Rollon
Mitsubishi
Mayr
ex
Rollon
Harting
NORD
Igus
Schmersal
Gimatic
Pepperl + Fuchs